Raffia tape and woven bag qualification

StageRecordCompare on this basis
Formulation PP lot, white masterbatch lot, filler and other mass fractions Same base and comparison conditions
Drawn tape Dimensions, actual dose, draw settings and observation window Use the agreed tape checks at matching conditions
Line stability Break count and elapsed time or throughput Same denominator and record any interruptions
Woven sack Fabric construction, coating or printing, approved white sample Same finished surface and fabric basis
Release Accepted tape and sack results; actual rate Only compare cost of qualified runs

Describe the tape and the finished sack

Give the supplier the PP grade, separate filler or other additives, target tape dimensions or linear density, fabric construction and whether the sack is coated or printed. Specify the customer-approved white sample and whether the inner fabric or the coated face is the relevant surface.

Preserve the settings that make trials comparable

Use a reference run with the same resin lot and documented formulation. Record actual candidate dose and its mass basis, approved draw conditions, line speed and the observation window. Count breaks over comparable elapsed time or material throughput. Log who changed which variable if a condition has to be adjusted.

Check tape and fabric at the right stage

Retain the drawn tape and finished woven fabric. Agree whether appearance will be judged on bare fabric or after coating and printing. Record outcomes for color, tape strength and elongation using the project's methods, and log breaks as observations. Investigate recurring events against the reference run before attributing them to a masterbatch.

Decide on a qualified bag rather than a white pellet

Sign off the required tape and finished-bag checks with the defined construction and dose. When fillers or other additive streams are present, enter them in the blend-cost comparison. If the buyer prices by bag or fabric area, compare the cost over the same accepted bag size and basis weight.

Common questions

Can I approve the white on an undrawn strip?

Use an undrawn sample for observation. The project approval should cover the drawn tape and the finished woven or coated surface specified by the buyer.

Should the filler percentage change between white-masterbatch trials?

Keep the filler stream constant for a direct pigment-grade comparison. If changing filler is the objective, record it explicitly as a separate formulation comparison.

Send your PP woven sack trial brief