Compare affected and accepted shade records

VariableLast accepted sampleFirst affected sample
Formulation and actual dose Record measured dose basis and formula revision Record values from affected time period
Gauge, production and material lots Record actual gauge, settings, resin and masterbatch lots Enter what changed and when
Viewing and physical reference Record lighting, backing and reference ID Repeat under identical setup before drawing a conclusion
White masterbatch sample pellets in a clear jar.
Newlane product reference; grade properties require documentation and trial confirmation. Original image

Standardize the comparison first

Use the same thickness, measurement or viewing method, light and backing. Check the physical reference has not been changed or damaged before assessing drift.

Trace both materials and processing

Record base-resin and masterbatch lots, actual formulation, time and line settings around the last accepted sample and first affected sample.

Log which variables changed

Compare the two samples and records side by side. A changed shade after a lot switch is a correlation; thickness, method and other production changes should be checked in the same review.

Define a controlled follow-up

Keep a hypothesis list and, with production approval, change one identified test variable at a time against the same baseline. Record the confirmed result or leave the cause unresolved.

Common questions

Can different light sources change the comparison?

Yes. Record and standardize the agreed viewing conditions.

What should be retained from each batch?

Retain identified pellets, relevant base resin and finished samples under the agreed plan.

Prepare my grade trial request